What TP347 / 347H is
Type 347 is 18Cr-10Ni stainless stabilized with columbium and tantalum at roughly ten times the carbon content. Like 321, it resists sensitization in the 800 to 1500 degree F range, but columbium carbides are more stable than titanium carbides, which improves weld-zone corrosion resistance and elevated-temperature strength. TP347H, with controlled carbon and grain size, is the standard austenitic grade for final superheater and reheater tube.
Chemical composition
| Element | Requirement |
|---|---|
| Carbon | 0.08% max (347); 0.04 to 0.10% (347H) |
| Chromium | 17.0 to 19.0% |
| Nickel | 9.0 to 13.0% |
| Columbium + Tantalum | 10 x C min to 1.10% max (347); 8 x C min (347H) |
| Manganese | 2.00% max |
Mechanical properties
| Property | Minimum |
|---|---|
| Tensile strength | 75,000 psi (515 MPa) |
| Yield strength | 30,000 psi (205 MPa) |
| Elongation in 2" | 35% |
Where it is used
- Final superheater and reheater tube in utility boilers.
- Refinery heater radiant and convection tubes, FCC and coker units.
- High-temperature hydrogen and hydrocarbon service.
- Chemical plant furnace tubes and heat exchangers above 1000 degrees F.
Ordering note
347H for pressure parts under ASME Section I requires specific heat treatment and grain size. Send the design code and temperature and we will make sure the certification covers it.
347 or 347H, OD, minimum wall, length, quantity, design temperature, grain size, and the ASME Section or licensor specification. Mention any stabilizing anneal or shot-peening requirement.